PublishedJournal of Electronic Materials · 2025

Faster cooling makes lead-free solder weaker but tougher

Faster cooling reduced strength and stiffness in simulated tin-based solders. SAC305 retained the highest tensile strength among the materials compared.

Tutorial Journal article

The problem

Solder joints experience repeated mechanical and thermal loads. Cooling history changes the structure that carries those loads.

What I did

LAMMPS molecular dynamics heated and cooled pure tin, tin–silver, and SAC305 models. A modified embedded atom method potential was used for tensile and cyclic loading after cooling.

6.42 to 5.60 GPaPure tin tensile strength

The drop as cooling increased from 2.5 to 100 K/ps shows that the rapidly cooled tin model carried less tensile stress before failure.

6.91 to 6.16 GPaSAC305 tensile strength

SAC305 weakened as cooling increased from 2.5 to 100 K/ps, while retaining the highest tensile strength of the three simulated materials.

108.96 to 97.65 GPaSAC305 Young's modulus

The decrease as cooling increased from 2.5 to 100 K/ps shows that the simulated SAC305 became less stiff.

What we found

  1. When cooling increased from 2.5 to 100 K/ps, pure tin tensile strength fell from 6.42 to 5.60 GPa.
  2. Over the same cooling-rate change, SAC305 tensile strength fell from 6.91 to 6.16 GPa and remained highest among the three materials.
  3. SAC305 Young's modulus fell from 108.96 to 97.65 GPa over that cooling-rate range.
  4. Toughness increased by 14.03% for tin, 12.87% for tin–silver, and 8.75% for SAC305.

Why it matters

The trends inform studies of how solidification conditions affect solder-joint reliability.

Recreate it yourself. Melt Sn, cool it at 10 and 100 K/ps with a MEAM potential, and compare strength and stiffness of the two solids. Open the tutorial →


Next case study · Selenium makes CdTe nanowires stronger and stiffer → · Back to Nanoscale mechanics research